    Other modes of applying the principle of the invention may be employed, change being made as regards the details described, provided the features stated in any of the following claims-, or the equivalent of such, be employed.I therefore particularly point out and distinctly claim as my invention: 1. A refractory composition,350-400t/h hard rock crusher plant comprising a pulverulent mixture of ground dry magnesian clinker and a small amount of dry substantially aluminum-free hectorite of the character of that from San Bernardino County, California.A refractory composition, comprising a pulverulent mixture of ground dry magnesian clinker and a small amount of dry gel-forming hydrous magnesium silicate.3. A refractory composition, comprising about 94 per cent of -100 mesh magnesian clinker, about 3 per cent of iron oxide, about 2 per cent of sodium nitrate, and about 1 per cent of hectorite.A refractory composition, comprising about 40 per cent of -4+15 mesh magnesian clinker, about 20 per cent of -15+100 mesh magnesian clinker, about 31.5 per cent of -200 mesh magnesian clinker, about 5 per cent of water-soluble sodium silicate, about 2 per cent of sodium carbonate, and about 1.5 per cent of hectorite.

    A refractory composition, comprising about 94 per cent of -100 mesh magnesian clinker, about 3 per cent of iron oxide, about 2 per cent of sodium nitrate, and about 1 per cent of a gelforming hydrous magnesian silicate.A refractory composition, comprising about 40 per cent of -4+15 mesh magnesian clinker, about 20 per cent of -15+100 mesh magnesian clinker,350-400t/h stone crusher plant about 31.5 per cent of -200 mesh magnesian clinker, about 5 per cent of water-soluble sodium silicate, about 1 per cent of trisodium phosphate, about 2 per cent of sodium carbonate, and about 1.5 per cent of a hydrous magnesian silicate.A process of plasticizing ground magnesian clinker, which comprises disseminating about 1 per cent of hectorite in about 94 per cent of 100 mesh magnesian clinker, about 3 per cent of iron oxide, and about 2- per cent of sodium nitrate.A process of bonding ground magnesian clinker, which comprises disseminating about 1.5 per cent of hectorite in about 40 per cent of -4+15 mesh magnesian clinker, about 20 per cent of -15+100 mesh clinker, about 31.5 per cent of -200 mesh clinker,40-60t/h hard rock crusher plant about 5 per cent of water soluble sodium silicate, and about 2 per cent of sodium carbonate.

    A process of bonding ground magnesian clinker, which comprises disseminating about 1 per cent of a gel-forming hydrous magnesian silicate in about 94 per cent of 100 mesh magnesian clinker, about 3 per cent of iron oxide, and about 2 per cent of sodium nitrate.A process of bonding ground magnesian clinker, which comprises disseminating about 1.5 per cent of a gel-forming hydrous magnesian silicate in about 40 per cent of -4+15 mesh magnesian clinker, about 20 per cent of -15 +100 mesh clinker, about 31.5 per cent of -200 mesh clinker, about 5 per cent of water-soluble sodium silicate, about 1 per cent of trisodium phosphate, and about 2 per cent of sodium carbonate.A process of the character described, which comprises disseminating in dry ground magnesian clinker a small amount of dry ground hectorite of the character of that from San Bernardino County, California, and subsequently gelling the dry hectorite by introducing water.A process of the character described, which comprises disseminating in dry ground magnesian clinker a small amount of dry fine gel-forming hydrous magnesium silicate, and subsequently gelling the dry magnesium silicate by introducing water.

To Top

Start a New Topic » « Back to the Diigo Community group